1、施工準(zhǔn)備
1.1防水材料選用和準(zhǔn)備
1.1.1一般選用高強(qiáng)度、低延伸的防水卷材,應(yīng)結(jié)合工程的實(shí)際情況,選用3㎜厚的Ⅱ類拉力≥400N、延伸率≥5%的黃麻胎體SBS改性瀝青防水卷材。
節(jié)點(diǎn)附加層應(yīng)選用氯丁橡膠改性瀝青防水涂料,要求固體含量≥43%,延伸≥4.5㎜,耐熱度為80℃時(shí)5h無(wú)流淌、起泡。
密封材料選用SBS改性瀝彈性密封膏,粘結(jié)性≥15㎜,耐熱度下垂≤4㎜。
1.1.2防水材料的質(zhì)量要求
所用的SBS卷材改性瀝青防水卷材、氯丁橡膠改性瀝青防水涂料、SBS改性瀝青彈性密封膏等均必須有出廠合格
CONTENTS
1, construction preparation ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 1
2, the construction process and sequence ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 3
3, method ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 3
4, detail treatment ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 4
5, water test ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 8
6, Technical parameters ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 8
7, the quality standard ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 8
8, quality control measures ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 9
9, quality defects prevention measures ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 9
10, product protection measures ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 10
11 Safety Precautions ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... ... 10
1, construction preparation
1.1 Selection and preparation of waterproof materials
1.1.1 General use of high strength, low extension of the waterproofing membrane, the project should be combined with the actual situation, using 3 mm thick, Class Ⅱ pull ≥ 400N, elongation ≥ 5% of the jute matrix SBS modified bitumen membrane.
Node should use an additional layer of neoprene modified asphalt waterproofing coating, required solid content ≥ 43%, extension of ≥ 4.5 mm, heat degree is 80 ℃, 5h free flowing, bubbling.
SBS modified asphalt sealing material used flexible sealant, bonding of ≥ 15 mm, ≤ 4 mm ptosis degree heat.
1.1.2 Water quality requirements of materials
Membrane used in SBS modified bitumen membrane, chloroprene rubber modified asphalt waterproofing coating, SBS modified bitumen flexible sealant Dengjun must have factory qualified